Introduction
Surface roughness influences plaque retention, wear behavior, and esthetics of interim restorative materials. Seashell-derived calcium carbonate represents a sustainable, aragonite-rich filler candidate for 3D-printable dental resins. The effect of shell-derived CaCO₃ on the roughness of 3D-printed composite resins after glazing and thermocycling remains unclear.
Aim
To evaluate the effect of shell-derived CaCO₃ incorporated at 1 wt%, 3 wt%, and 5 wt% into a CRS composite resin on the surface roughness (Ra) of 3D-printed specimens at the unglazed stage, after glazing, and after thermocycling.
Materials and Methods
Seashells were collected, cleaned, dried, and ground into powder. The mineral phase of the resulting powder was characterized using X-ray diffraction (XRD), which identified aragonite. Shell-derived CaCO₃ was incorporated into CRS composite resin at concentrations of 0 wt% (control), 1 wt%, 3 wt%, and 5 wt%. Disk specimens were fabricated using an Asiga 3D printer and subsequently post-cured under nitrogen using an Otoflash unit. The specimens underwent surface polishing, glazing, and thermocycling (5,000 cycles between 5 °C and 55 °C). Surface roughness (Ra) was measured using a Taylor Hobson profilometer at three stages: before glazing, after glazing, and after thermocycling. Twelve specimens were evaluated per group, and results were presented descriptively as mean ± standard deviation.
Results
At the unglazed stage, the 3 wt% CaCO₃ group showed the highest mean surface roughness (2.60 ± 0.62 µm). Glazing reduced mean roughness in all groups to a range of 0.59–0.78 µm. After thermocycling, mean Ra values converged and ranged from 0.48 to 0.54 µm across the groups. Inferential significance testing was not provided in the source dataset; therefore, the findings were presented descriptively.
Conclusion
In this descriptive dataset, shell-derived CaCO₃ incorporation influenced the initial surface roughness of the 3D-printed interim restorative resin, with the 3 wt% group showing the highest unglazed Ra values. However, glazing markedly reduced roughness in all groups, and after thermocycling the mean Ra values became comparable. These findings suggest that finishing and aging procedures may play a major role in determining the final roughness of CaCO₃-reinforced printable resins.